Stable Feed Grade, Stable Flotation Recovery

Ask any flotation plant metallurgist what they would fix first, and most will say feed stability. Collectors, frothers and cell hydrodynamics are all tuned to a target feed grade and particle-size distribution. When the feed swings — harder ore, higher grade, more clay — the circuit runs off-peak for hours while operators chase it.

The mathematics are unforgiving. In a porphyry copper circuit, a feed grade swinging between 0.4% and 0.7% Cu within a single shift typically costs 1–3 points of recovery versus steady-state operation, because reagent dosage and mass pull are always chasing the last sample. Over a year, those points are worth more than most expansion projects.

The fix is usually upstream, not in the flotation cells: a disciplined mine plan, an honest stockpile strategy, and crushing-plant blending ahead of the mill. Even a simple two-finger stockpile system, reclaimed alternately, can cut feed variance by half.

This is where our two businesses meet: we engineer grinding and flotation circuits for stable operation, and we trade ores and concentrates, so we see feed-stability problems from both sides. If your recovery fluctuates with the blast schedule, talk to us — sometimes the cheapest recovery project is a blending pile and a loader operator who follows the plan.

Have a parcel to sell, or a plant problem to solve? Talk to our team.

Get a Quote